Heterogeneously Nucleated
Homogeneously Nucleated
2 Blocking T¹s: Fe, Fe oxide
H = 200 Oe
Field-cooled, Zero field-cooled Magnetization
7.0 ± 0.8 nm
11.2 ± 1.0 nm
0.01vol. %
Blocking Temperatures